PETG has always been more fraught than PLA for me but as of late it just looks like a mess.

I’m just trying to do calibration at this point and I’m getting this mess on the pressure advance test in Orca Slicer.

https://imgur.com/a/zbEn5FR

I get so much stringing, boogers, and just terrible prints. It didn’t used to be this bad. Any tips?

I’m using a Snapmaker Artisan.

  • peregrin5@lemm.eeOP
    link
    fedilink
    English
    arrow-up
    1
    ·
    7 hours ago

    I’m using an Orca profile for the Snapmaker printer but other than that I’m not sure. Kind of just trusting they set that part up correctly.

    • scytale@aussie.zone
      link
      fedilink
      English
      arrow-up
      1
      ·
      7 hours ago

      Yeah it should be, how well did it go last time you printed Pla? There are so many things that can go wrong, just trying to eliminate some. (Drying filament never hurts so long as you actually have a dryer and don’t just stick it in the oven and hope for the best)

      • peregrin5@lemm.eeOP
        link
        fedilink
        English
        arrow-up
        1
        ·
        5 hours ago

        PLA worked fine. I just bought and loaded some new PETG btw and it prints pretty well so I think everyone is right that the filament is just really old/wet.

        Threw 80 bucks out to get a dryer.